Trade fair: meet us at Adhesives & Bonding Expo Europe, 10–12 November 2026, Messe Stuttgart, Hall 1, Booth 1001. Details & appointments →
Full-chain cloth & adhesive tape manufacturer · Since 2020
3 models

Conductive cloth tape (EMI) — technical datasheets

Plain-weave metallised conductive cloth + conductive adhesive. EMI/RFI shielding and grounding of cable bundles, connectors, flexible circuits and display modules.

Datasheet revision 2026-08-19

BEP212-2110SS

PropertyValueMethod
ColourBlack—
Total thickness0.11 ± 0.01 mm—
Master-roll width1270 mm (master roll; slit to spec)—
Peel adhesion, 180°≥ 800 gf/inch (180°)—
Holding power≥ 48 h—
Service temperature80 °C—
Ball tack≥5 (ball no.)—
Resistance≤ 50 mΩ—
Flame behaviourNot flame retardant—

LV 312 class: not classified. We do not estimate one from the values above — what a classification needs.

Request this datasheet & a sample →

Datasheet revision 2026-02-28

EP208-2110SS

PropertyValueMethod
ColourGrey—
Total thickness0.08 ± 0.01 mm—
Master-roll width1270 mm (master roll; slit to spec)—
Peel adhesion, 180°≥ 800 gf/inch (180°)—
Holding power≥ 48 h—
Service temperature80 °C—
Ball tack≥5 (ball no.)—
Flame behaviourNot flame retardant—

LV 312 class: not classified. We do not estimate one from the values above — what a classification needs.

The EP212 and BEP212 datasheets state ≤50 mΩ and that unit is confirmed correct (owner, 2026-10-23). This model’s datasheet prints ≤50 MΩ — a typographical error being corrected at source — so resistance for this grade is quoted on the signed datasheet rather than here.

Request this datasheet & a sample →

Datasheet revision 2026-08-19

EP212-2110SS

PropertyValueMethod
ColourGrey—
Total thickness0.11 ± 0.01 mm—
Master-roll width1270 mm (master roll; slit to spec)—
Peel adhesion, 180°≥ 800 gf/inch (180°)—
Holding power≥ 48 h—
Service temperature80 °C—
Ball tack≥5 (ball no.)—
Resistance≤ 50 mΩ—
Flame behaviourNot flame retardant—

LV 312 class: not classified. We do not estimate one from the values above — what a classification needs.

Model-level test reports: A2250975736101001E

Request this datasheet & a sample →

The technical data on this page is reproduced from the manufacturer's datasheet for the model named. It is for reference only and is not intended as a basis for product acceptance; for a special application, test and confirm before use.

Best-before 6 months from despatch. Store at 25 °C / 65 % RH in a cool, ventilated place, out of direct sunlight.

LV 312

LV 312 classes — what we can show, and what we cannot

Two of our harness grades carry class designations on their own datasheet, with the test standard printed next to each value. The rest of the range does not, and we do not estimate a class from a peel figure or an in-house temperature reading.

ModelPropertyValue on our datasheetTest standard cited
K8030temperature−40 °C to +105 °CLV 312
K8030noise dampingClass C — 5 to ≤10 dBLV 312
K8030scrape abrasionClass B — 100–499 cyclesISO 6722
K8030flammabilityClass B — self-extinguishingISO 3795
K8030peel adhesion≥ 3 N/cmEN 1939
K8030tensile strength≥ 30 N/cmEN 14410
K8030elongation at break≥ 20 %EN 14410
K75100-00temperature−40 °C to +105 °Cdeclared on the TDS; test standard not printed
K75100-00noise dampingClass A — ≤2 dBdeclared on the TDS; test standard not printed
K75100-00burn rate≤ 100 mm/mindeclared on the TDS; test standard not printed

Why most models show “not classified”

An LV 312 class is the result of a specified test, not a property you can read off a datasheet. The acetate, nylon and conductive grades below report a 80 °C service temperature measured in-house on our own instruments — that is not an LV 312 temperature class, and we do not print one. Classification is done per tape model, on the construction actually supplied.

The four axes a harness drawing asks for

Temperature class, scrape abrasion (cited as ISO 6722 on our classified grade, and only meaningful with the mandrel diameter next to it), noise damping in dB, and flammability (cited as ISO 3795). Each is measured separately on the same model — a high temperature class says nothing about abrasion. Peel and tensile on those reports are cited to EN 1939 and EN 14410.

Need a class on a model that has none yet?

Tell us the model and the class your drawing calls for. We submit the construction for test and send you the report with the model number on it — we do not transfer another grade’s result onto it.

Request a classification & report
Compliance

Third-party reports covering this construction

Each report covers the sample that was submitted. Where the report names a model number it is model-level; where it names a product category it covers the construction, and we say so rather than attaching it to a single model.

All test reports, with methods and limits →

Product pages

What these models are sold as

Need a width, colour or liner that isn’t listed?

Master rolls are slit to your width, and we build to a drawing. Send the model and the dimension you need.

Request a quote & samples